- - By RayZ Date 03-29-2011 16:48
:grin: Hi Everyone,
I'm a little new to Inspection. I just wanted to ask, in AWS D1.1 table 6.1 (6) there’s a wait time of 48Hrs for visual inspection. Does the same hold true for UT & RT? If so where is it in the specification?
Parent - By L51174 (**) Date 03-29-2011 17:03
The wait applies to specific steels only. The info you're looking for can be found.... by reading the applicable code. It's in Sec 6, Inspection.
Parent - - By jwright650 (*****) Date 03-29-2011 18:20
Like L51174 stated, there are a few grade 100 and grade 100W steels like ASTM A514, A517, A709....that require the waiting period.(See Clause 6.11 2nd paragraph)
Parent - - By eekpod (****) Date 03-29-2011 20:08
otherwise it should be cooled to ambient temp, or close.
Parent - - By 803056 (*****) Date 03-29-2011 22:32
Took the CWI using API for the open book portion?

Al
Parent - - By jwright650 (*****) Date 03-30-2011 11:21
Al, that very question appeared on my CWI exam back in "the day" when I took it.
Parent - - By 803056 (*****) Date 03-30-2011 15:02
That's my point John. The practice questions provided to those individuals taking the D1.1 session still includes that very question.

Best regards - Al
Parent - By 99205 (***) Date 03-31-2011 06:29
that question was on the test I took.
Parent - By RayZ Date 03-31-2011 15:57
Thanks found it right where you said :smile: