Hi Everyone
I have a part which is customer specified to preheat to 450 F and then wrap in a Thermal Blanket until ambient. Can someone help me with what an appropriate product for this might be? A Supplier?
Thanks in advance
By
TimGary
Date
04-08-2011 18:10
K-Wool, Rock Wool, Thermafiber, Ceramic Blanket, etc
many names from different suppliers...
http://www.sealproweb.com/kwool.html
http://www.certainteed.com/products/insulation/stone-wool-(rock-wool
)/317389
Tim
By
bIGwIRE
Date
05-18-2011 17:06
http://thermalproductsco.thomasnet.com/viewitems/thermal-products-textiles--1045/siltemp-silica-fabrics
This is the product a lot of shops around here use. Works pretty well for a little less $.
Topic
Welding Industry
/
Technical Discussions
/ Post weld heat treat (thermal blankets)
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill