![](/mwf/attachments//avatars/3040-3756.png)
Download the .pdf from this link below to your desktop, and then open up the document and look for page 7 (Shown at the bottom of the page) which is really page 15/23 of this document.
![wink :wink:](/f2/epx.png)
![cool :cool:](/f2/epx.png)
This will give you an idea of what to look for in a WPS written to AWS D17.1 from NASA.
http://standards.nasa.gov/documents/viewdoc/3314906/3314906 There's a lot of useful information in this NASA .doc to guide you in developing a WPS that would satisfy the requirements for AWS D17.1:
http://mmptdpublic.jsc.nasa.gov/prc/7187C.docThat's it for now... If I find more, I'll post it up later.
![roll :roll:](/f2/epx.png)
![lol :lol:](/f2/epx.png)
![wink :wink:](/f2/epx.png)
![cool :cool:](/f2/epx.png)
Respectfully,
Henry