- - By Billyboy (*) Date 11-22-2011 14:22
Hi Fellas, I'm trying to help a welder prepare for his CWI exam and ran into a problem with a practice question.  I have searched for far to long and now need to swallow my pride and ask for assistance.  If you could please just give me a hint as to a key word to search or the like, instead of the exact location I would be very appreciative.  It seems like such a simple question I am feeling like a heel!! Here goes:

"What is the maximum gap permitted between the back side of a butt joint and its backing bar?"
Parent - - By L51174 (**) Date 11-22-2011 15:06 Edited 11-22-2011 15:18
Figure 5.3? Nope scratch that, sorry. 5.22.1.1
Parent - - By Billyboy (*) Date 11-22-2011 15:19
AAAAHHHHHH!!!!!!!  :eek:  :eek:  I read over it a hundred times!  Thank you!!!
Parent - - By L51174 (**) Date 11-22-2011 15:32
You're welcome, I answered off the cuff with figure 5.3, something you should never do on a test, and I was way off. So I feel kinda dumb too if it makes you feel better :red:
Parent - By rshanks (**) Date 11-22-2011 20:11
5.22.1.1, AWS D1.1  +1/16
Parent - By Duke (***) Date 11-23-2011 02:46
"assembly"