Our Indian Project Customer is insisting to write WPS again for 316 even we prequalified for 316L  as per both grades are under same family as per AWS D1.6 under scopes. Is there are any clauses in AWSD1.6 under base metal classification requires to do so ?. Kumar, bhaav23@gmail.com
Parent - By ozniek (***) Date 11-25-2011 09:28
Hi bhaav23

I would suggest that you re-post this in the D1 or Technical boards. Will probably get more people looking at it there.