- By gross Date 12-12-2011 07:02
Hi averyone, we braze blades with heneycomb, both from nickel alloys, the problem is, after vacuum furnace we have braze metal droplets on airfoil. We dry the brazing paste before furnace loading minimum 3 hours. Maybe someone can give some tips. Many thanks.