- - By brucearnold Date 12-17-2002 21:27
I am trying to locate a published paper on the welding of C-276 (N10276) to 304 (S30400). I am aware of the problems that will occur, but I need a published paper from another source to convince...Links would be helpful as well...

Regards,
Bruce
Parent - - By MBSims (****) Date 12-19-2002 13:46
How about this:

http://www.haynesintl.com/mini/C276s/C276.htm

Marty
Parent - By brucearnold Date 12-19-2002 19:59
Thank you for the reply, the link appears to be down. I will try again later...

Bruce