- - By RYAN HANAGAN Date 02-06-2012 12:43
We have 1/4 1/4 overlay plate and trying to butt weld together.  The weld keeps splitting dead center.  Any help with stoping the cracking would be great.  We are using 7018 rod.
Parent - By DaveBoyer (*****) Date 02-07-2012 04:31
You may get more response posting this in the "Shop Talk" or "Technical" sections.

This section being the "Resistance Welding" section may not be read by the people with the answer to Your question.

It will also help if You mention the specific alloy of the material, and any pre or post heating You have tried.