D1.1 2010 Table 4.10 note (h). Anyone notice the discrepancy there? The reference must be a misstype. I don't see the reference in the notes located within the sections listed as 4.25 and 4.26. These sections do not address the concern at all. Nor does it appear to be directing us to the Figures. This is applicable to fillet welds on pipe and T, Y and K connections. Anyone have input on this? Question is: where is note (h) attempting to point us to? sections, tables or figures or a section not apparent to me?