Dear all,
I like to ask 2 questions:
1. We have a WPS qualified IAW ASME IX using SAW flux/wire class F9A0-EF3-F3. May we substitute this cons with F10A6-EF3-F3 IAW ASME IX?
2. We have a WPS qualified IAW ASME IX using SAW flux/wire class F9P0-EF3-F3. May we substitute this cons with F9P6-EF3-F3 IAW ASME IX?
Impacts apply in both cases.
Rgds