Well I understand that but a Coupon Test Report should prove that WPS and as long as I have that documentation, I should be able to weld production pipe following that WPS. Section IX is where you see PQR's, not 1104 thus the question, where is the section in 1104 that specifically states you have to have a PQR and a WPS... agree? Read over 5.2 RECORD again....