The little wheels that come with the circle cutting attachment left a lot to be desired, so I made this.  The plasma head fits snugly in the bore, eliminating the need for setscrews, and I just drag edge of the adapter along a straight edge.  I couldn't place the axis of rotation right over the nozzle, so there are two different offsets I need to use depending on if I am beveling left or right, but it works for its intended purpose, which is to make compound miters on rectangular tube.
Parent - - By WeldorJoe (*) Date 05-04-2012 17:56
Neat.....coming from a small job shop background I can appreciate the workmanship.
Parent - - By devo (***) Date 05-05-2012 01:19
you mean the dykem still visible on the bottom piece?
Parent - By WeldorJoe (*) Date 05-08-2012 15:34
Never even noticed....we used to make a lot of our own custom equipment also