Dear Experts
API 5L X52-Group II & API 5L X65-Group III materials
Seek your expertise
T-Y-K FP Weld connections
Weld Process - SMAW
PQR qualifed with API 5L X52 using SMAW -( Root run-LB52U / Fill & Cap-LB52NS- AWS Classifications- E7106- F4 ).
Can i use this PQR to weld T-Y-K Joint ( Main tubular- API 5L X52 & Bracing - API 5L X65 )?
What is the most appropriate electrode( E7016 or E8018 ) to weld this T-Y-K FP Joint?