- - By reta (*) Date 11-07-2012 13:43
I need a quickly answer, please

Code ASME IX:  a welder was qualified in a double groove weld, He is qualified for fillet weld ?. All variables are the same
Parent - - By ssbn727 (*****) Date 11-07-2012 23:15
More details needed please!!!

A drawing would help!

Respectfully,
Henry

Btw, Do not ever expect a quick answer to a question such as yours in here without more details understand???
That's not how we roll here!
Parent - - By Shane Feder (****) Date 11-08-2012 00:29
Henry,
Belated Happy Birthday for yesterday - home on R&R in Thailand so don't get on the internet very often.

Reta,
Yes, the welder is qualified - see QW 452.6,
Regards,
Shane
Parent - By ssbn727 (*****) Date 11-08-2012 02:09
Thanks Shane!

So you know this person? okay then but, I hope they know that if you're not available they'll have to give more details in order to get an answer.:cool:
Also, just so they know, I'm not trying to give them a hard time, I'm just describing to them how it's done here so please do not get offended Reta...

Enjoy the R&R Shane! You deserve it friend!!!:wink:

Respectfully,
Henry
Parent - - By congnt.biz Date 11-08-2012 02:57
Yes Sir,

A welder who have been qualified by any groove weld shall be qualified for fillet weld with all base material thicknesses, fillet sizes and diameters. So in your case, if all variables are the same so I would like to confirm that the welder you mentioned is qualified for fillet weld.

Make a reference to ASME IX QW-452.6 you will find your answer!

Best regards,
Parent - - By reta (*) Date 11-15-2012 18:51
I went to  section QW-402 and it said a double welded groove weld is considered welding with backing
Parent - - By 46.00 (****) Date 11-17-2012 07:14
reta, QW-452.6 is quite clear. Whether a groove weld is backed or not, is irrelevant! Shane & congnt.biz are correct!
Parent - By reta (*) Date 11-17-2012 14:51
thanks to everybody, now is clear