I have an old drawing that references a electrode "AWS RG65" which is also cross referenced as Linde Oxweld 32. Does anyone know if this is still in existence? If so were can it be bought?
AWS A5.2 specifies rods for gas welding, which is what you have there, and most manufacturers would make a rod that conforms to RG65, however, if you don't want to use gas welding, you would want to switch electrode types also.