- - By scmait (*) Date 02-10-2003 17:20
I have an old drawing that references a electrode "AWS RG65" which is also cross referenced as Linde Oxweld 32. Does anyone know if this is still in existence? If so were can it be bought?

Thanks,
SCMait
Parent - By Niekie3 (***) Date 02-10-2003 17:41
The "RG" is a reference to oxy-fuel gas welding filler. The AWS spec is AWS A5.2. While I do not have anything to do with this welding process, I believe that the fillers should be readily available.

Regards
Niekie Jooste
Parent - By RonG (****) Date 02-10-2003 17:43
ESAB