what´s the standard or certification I should to use for qualification a reparation within cast iron welding? and, can I to use this standard for qualification welding for maintenance?
I have found AWS D11.2- "Guide for Welding Iron Castings" to be a very good source for direction and implementation of WPS's, PQR's and WPQ's when qualification of welding iron castings is required.