- By russelsl Date 08-29-2013 17:04
Does anyone concur? If I qualify a welder for fillet welds via a 3/4" thick groove weld test, per Table 4.3 (note d) the qualified deposited thickness range for fillets is "1/8" min to Max to be welded"? That is the way it looks to me although I find it odd. D1.1 and Section IX groove weld tests qualifies the welder for all fillet sizes.