Up Topic Welding Industry / Metallurgy / S/S concrete anchor bolts
- - By kcd616 (***) Date 09-18-2013 19:23
So I am in the market for new rotary hammer drill and go to the Hilti site to check first. and see they have anchor bolts, so check the price on them.
I am shocked to see stainless steel anchors.. did some work for both Bechtel and Fluor and they were just OCD about s/s and concrete.
has something changed?
Thank you for your time and consideration.
Sincerely,
Kent
Parent - By Dualie (***) Date 09-20-2013 05:26
i curse them for having those in the catalog.     you would be amazed how many times dumb engineers spec SS wedge anchors for the most mundane stuff.