- - By Diver Date 02-28-2003 21:50
I am a commercial diver with Underwater G3 Certification. My certification papers do not show a experation date if you will!! How long does such a certification hold validity? Thanks for the help.
Parent - By MBSims (****) Date 03-01-2003 05:01
If you were certified to AWS D3.6, I believe they are effective indefinitely as long as you are welding at least every 6 months and your employer is tracking your use of the process. Otherwise, they would expire 6 months from the last date the process was used.