Dear Experts Hi Is There any standard WPS for SMAW Carbon Steel to Austenitic Stainless Steel ( ST37 to A304 , THK: 10mm , V Groove ) ? If yes do send me the Document No. .
You might like to look at this: B2.1-1/8-228:2002 (R2013) (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL (M-1/P-1/S-1, GROUPS 1 or 2) TO AUSTENITIC STAINLESS STEEL (M-8/ P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, E309(L)-15, -16, or -17,