- - By Tomwalz (*) Date 01-16-2014 20:35
Immediate need for Plymetal, (trimetal, Sandwich) material based on 49% silver alloy with Manganese ( BAg-22) and Nickel.
Parent - By tinovolpe Date 03-18-2014 16:51
Have you tried Lucas Milhaupt? I think they offer various types of plymetal