High strength steels are harder to magnetize, but once they are, it is harder to demagnetize them.
If the plate was handled with a magnetic lifting device, the retained field could be bothersome and may require demagnetization.
The subject has be covered in several past threads. Do a search and you will have plenty of opinions and recommendations on the subject. Good luck.