- - By goldybowen21 (**) Date 05-22-2014 13:37
I am making prequalified joint packages for companies and I have them all done except a few of them don't have pass and layer sequences in the WPDS, so I'm wondering if it is a prequalified joint, does it need a pass and layer sequence in the WPDS and also if it does where do I find them?
Parent - - By pipewelder_1999 (****) Date 05-24-2014 11:39
I am not sure of any code requirement that would require a pass and layer sequence however that doesn't mean it's not necessary or a good idea. However, if it were,  it would be driven by the company doing the welding and they would provide that information. 

Gerald Austin
Parent - By goldybowen21 (**) Date 05-26-2014 13:52
thanks, very helpful!
- By goldybowen21 (**) Date 06-06-2014 18:43
NEW QUESTION- Resistance welding WPDS packages For stainless steel (304)
.037
With a range of thicknesses 16Guage – 22guage.

JUST LOOKING FOR SOMEWHERE TO FIND INFO ON RESISTANCE WELDING.