Dear Experts
31) A change in groove type (e.g., single-V to double-V), except qualification of any CJP
groove weld qualifies for any groove detail conforming with the requirements of 3.12 or 3.13
Query.
PQR qualified with Single-V in 3G Position ( CVN tested -40 dec C / Weld Process-FCAW/ Test Coupon thk-25,4mm).
Can i weld all groove detail as listed in 3.12 OR 3.13 conforming to groove configuration details( Root Gap, Root Face, Bevel Angle)?
Does any one have AWS Interpretation in this subject?
Sincerely appreciate prompt answer