- - By vvvmaac Date 06-22-2014 13:37
I think there's a mistake on Fig.  4.60 on page 4-42. Welding technologies book.
Weld specification is given as 3/8" and then as 5/16" for the same member,  or I'm reading it wrong?

Thanks for the help.
Parent - - By Milton Gravitt (***) Date 06-22-2014 14:58 Edited 06-22-2014 15:03
You are looking at the welding of the stiffeners when you looking at section A-A the other view is looking at the flanges on each end you also looking at the welding on the web.
Parent - By vvvmaac Date 06-23-2014 02:46
Thanks for the answer.
Parent - - By vvvmaac Date 06-23-2014 19:26
So,  3/8 weld size for flanges to ends,  and 5/16 web to flanges. Right?
Parent - By Milton Gravitt (***) Date 06-23-2014 22:43
The 3/8 weld is on the flanges at both ends and the 5/16 is on both flanges the 1/4 is on the stiffeners that is the way I see it, but I could be wrong also. There is more prep on this part to.

                M.G.