- By Funfax (*) Date 10-27-2014 06:24
Hi All

I have some question about qualification stud weld.

- I have the two studs which same diameter and geometry but the length is different. I don't know that the length of the Stud this essential variable. I must be generate 1 or 2 PQR ?

Sorry for my english

Thank

Regard,
Polra