/ Diesel fuel tank ends
By
Smooth Operator
Date
07-24-2015 22:51
Need to build a new diesel fuel tank for my crane......Can"t seem to locate formed ends 22" x 22" in either steel or aluminum ......Anybody know of a supplier I can contact?????? Thanks in advance....
By
CWI555
Date
07-26-2015 15:38
Putting aside legalities, why don't you do an orange peel?
By
Superflux
Date
07-26-2015 18:04
Those orange peels are an awesome way to spend an afternoon.
They are a lost art and you had better lay out and cut Acurately!
By
kcd616
Date
07-26-2015 22:57
flux
how true
made more than my share
sincerely,
Kent
By
fschweighardt
Date
07-27-2015 02:00
These dudes have a ton if you want round heads
http://www.cmforming.com/
By
Dualie
Date
07-28-2015 01:41
http://www.allenjacfueltanks.com/
http://www.clevelandtank.com/aluminum-fuel-tanks.html
Topic
Welding Industry
/
General Welding Discussion
/ Diesel fuel tank ends
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill