Up Topic Welding Industry / Technical Discussions / A simple questions.
- By jiunsi Date 04-07-2003 20:37
I need weld a T joint in fillet weld, in a base material ASTM A 36 of 1/4" of thickness. If I use when the process SMAW, with filler metal E-6010, and size leg is 1/8" for one side and 5/16 for other. ┬┐This is a prequalified procedement?.

Thanks