- - By rakeshka Date 10-20-2015 04:27
We need to qualify a WPS to weld SS 410S to A387 Gr.22 as per AWS. We have been using E309Cb for 410S and E9018-B3 for A387 Gr.22, but can anyone suggest which consumable can be used for the combination in SMAW. And what preheat temperature can be applied for the same.

Thanking in advance,

Rakesh
Parent - By kcd616 (***) Date 10-20-2015 12:28
SMAW????????????
why????????????
EOR needs to rethink the welding process used, if they can even think
(back to Kent normal and bashing engineers)
as far as preheat, I would be more concerned with post heat
so try again,
and explain why this is being done this way
then the solution will appear
sincerely,
Kent