- - By MRWeldSoCal (***) Date 11-09-2015 18:02
I work for a Testing lab and we recently updated to a nice digital microscope.  Here are some of the welds that come through.

J

http://imgur.com/a/6ZivJ
Parent - By aevald (*****) Date 11-09-2015 18:26
Awesome photos! thank you for sharing here. Best regards, Allan