I have welder qualification base on aws d1.1 CJP with multiple process smaw(root) + fcaw-G(fill+cap).
question: 1. welder can weld from root to capping with process full smaw refer to aws d1.1?
                2. welder can weld from root to capping with process full fcaw-g (with backweld smaw) refer to aws d1.1?
since i cannot find this clauses on aws d1.1.
Parent - By Superflux (****) Date 12-05-2015 15:51
Not a D1.1 expert, but Unless proven otherwise I think it would all be good as long as it is one of the prequalified joint designs (not open root) and maximum deposit thickness isn't exceeded.
- By 803056 (*****) Date 12-05-2015 17:56
AWS D1.1 includes no provisions to permit using more than one process on a single test assembly.