Anyone here who can give some guide line of where I can go to search deeply in the topic of hard surfacing (applying high alloy welding materials onto some softer base materials to changes the surface characterictics to harder surface). Any ideal on this issue is highly appreciated. Thanks in advance for all the advice.
Parent - - By n5uzt (**) Date 04-13-2003 16:50
the http://www.thermadyne.com/stdy/index.asp?div=stdy best people on hardfacing are stoody go to this link above or you can do a search on thermadyne or stoody.
Parent - By kk_chiong (*) Date 04-16-2003 15:31
Thanks for your advice and I will look into this web site.