- - By avekaria Date 01-04-2016 21:01
Hello,

We are attempting to qualify a WPS using ASTM A148 cast plate.
Note 3, in this figure specifies that the dimensions are minimum

The diagram suggests that the total dimension of the plate be at minimum 14 in x 30 in
How flexible are these dimensions if not all plates are required?

Thank you
Parent - By 803056 (*****) Date 01-04-2016 21:44
If the dimensions are listed as minimum, they can be anything larger.