Hi everyone,
I'm going to make a WPS with base metal ASTM A709 HPS 70W [HPS 485W] but so far haven't known proper consumables.
Mechanical Specification:
- Minimum Yield: 485 MPa
- Tensile Range: 585-760 MPa
Chemical Compositions (Maximum):
- C: 0.11%
- Mn: 1.10-1.35
- Si: 0.30-0.50
- P: 0.020
- S: 0.006
- Cr: 0.45-0.70
- Ni: 0.25-0.40
- Mo: 0.02-0.08
As I know, critical compositions are C, Mn, Cr
Please let me know if there is any advise, I intend to use Hyundai brand. And it's ok if there is another brand (Kiswel, etc).
Thanks.