By HJLBX
Date 06-25-2016 06:10
D1.1\1.1M:2015
Table 4.3
p. 123
Note (b)
"...,the butt joint shall have a temporary restrictive plate in the plane of the of the square face to simulate a T-joint configuration."
Normal to surface of butting members adjacent to the weld groove - to simulate - for example - an intermediate web stiffener to flange ?