in studying for cwi exam I came across root face dimensions of 1/4 inch max but as fit tolerances of plus or minus 1/16 am I right to assume those tolerances do not apply in this case and the joint should be 0 to 1/4 . Going as high as 5/16 is not an option? As always thank you for your time in answering my question.