I work in the oil and gas industry, where most downhole tools are made of 4145H modified high tensile steel. I was looking into welding of this material so searched for a matching ASTM equivalent but was unsuccessful can anyone help with this? Also any information on welding electrodes or pre/post heat treatment will be helpful.
Parent - By 803056 (*****) Date 07-19-2016 20:29
Try ASTM A182 for forgings, A217 for castings, and A234 for weld fittings

Al
Parent - By js55 (*****) Date 07-20-2016 13:28
There are ASTM standards such as A519 that include the AISI steels used in oil and gas. I would recommend you contact your materials distributor and see if he can help.