- By Toey TNDT (**) Date 12-20-2016 16:46
Dear All ,

I have a question about pipe Cold bend . In Table 841.2.3-1 show Minimum Radius of Bend in Pipe Diameters

i supposed Pipe   ⌀ 12 " have to Minimum Radius of Bend in Pipe Diameters is 18D

how i calculate and measurement at field , i compared formula in pipeline handbook but i don't know which one is true

Please recommended