I want to weld A387 Grade 11 with Cor-ten Material. can anybody describe it with code reference if Plate thickness of A387 p11 is 25mm and Corten material thickness is 18mm. which mechanical test required during PQR, and which technique use for sound weld,
Parent - By Lawrence (*****) Date 05-10-2017 12:50
Hi Rizu.

Cor-ten or Weathering Steel has been a topic on the forum many times.

Much depends on your actual required specifications.

However you can do a search on the forum here (search function) and you can review the many conversations others have had.

AWS D1.1 has some specific data on Weathering Steels.
The D1.1 index has numerous references for design (clause 2), prequalified filler data (clause 3), and fabrication (Clause 5).
- By 803056 (*****) Date 05-10-2017 12:59
What is the application and what is the applicable code (if one does apply)?