- - By Len Andersen (***) Date 05-31-2017 16:54
Have Five Patents In Thermite in Welding was asked about thermite welding on shaft on machinery. Internet says 14 inch done. Input sought.
Sincerely
Len Andersen Engineer IGTI – ASME Presenter of Paper at
Power & Energy Conference June 26-30, 2017 Charlotte, North Carolina
Power Energy 2017-3191 // New Tech Combined Cycle Gas Turbines (CCGT) - Analysis of Water Swirled Into Gas Turbine Technology 29 June
len@lenandersen.com
HP Securemail
914-536-7101
/ 914-237-7689
(H) / 800-428-4801
USA
POB 1529 / NYC 10116-1529
Caller Box NY NY ~1299 USD / year
Parent - By 46.00 (****) Date 05-31-2017 21:18
In theory, I would not see a problem with 14 inches of thermite welding. Some more info would be good!?
Parent - - By Len Andersen (***) Date 06-02-2017 18:57
Thank you for the reply. Read the article - looked into it more! It was 1911 use for shaft on a ship. Things have changed.
Parent - By mcostello (**) Date 06-04-2017 02:54
Would slag inclusions be a problem?