- - By Seymour86 (*) Date 10-05-2017 13:48
Hi all I have just been tasked with getting everything in order to have a few guys here at our job qualified for tack welding with the GTAW process. I see everything I need in D1.1 to qualify down to 1/8"  but I don't see anything in D1.3 for qualifying tack welders for thicknesses less than 1/8".  Just wondering if someone could point me in the right direction to get some guys qualified to tack sheet steel <1/8"? thanks!
Parent - By 803056 (*****) Date 10-06-2017 12:36
No distinction is made between a tack welded and a welder in the standard. The person is a welder or he isn't.