Lim Hyunsub
Date
11-01-2017 07:03
Please help
Is it possible to apply radiographic inspection for t, k, and y joints?
If so, is it mandatory on codes or standards?
By
803056
Date
11-02-2017 19:43
Yes, DWE and DWV or DWE and SWV. In some cases, if the tubular member is large enough and there is sufficient access; SWE and SWV.
Al
By
Lim Hyunsub
Date
11-03-2017 01:38
Thanks.
But in case of SWE and SWV in a large member, isn't it hard to place the film on bead?
Especially on the part of 45degree.
By
803056
Date
11-03-2017 02:33
There are always challenges and problems to solve.
Al
By
Joey
Date
11-06-2017 04:37
It may be possible to you but not possible to your RT Technician.
Your trusted RT technician is the best person to give advice on your needs.
If all people can shoot well, then nobody will patronize a photography studio.
Topic
Welding Industry
/
General Welding Discussion
/ RT on TKY joint
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill