- - By ABUMECH Date 12-10-2017 10:44
DEAR ALL,
ANY ONE THERE TO HELP ME!!!
I HAVE 3 QUESTIONS
1.HOW TO WRITE WPS FOR A36 TO SS316 WELDING, WHAT ARE ALL THE THINGS REQUIRED TO CONSIDER IS IT POSSIBLE TO WRITE WITH ASME SEC IX PQR POSSIBLE???
2.WHAT IS PREQUALIFIED WPS IS IT IS POSSIBLE TO WRITE FOR THIS CONDITION???
3.WQT WITH ASME SEC IX WPS IS POSSIBLE FOR AWS D1.1 WELDER QUALIFICATION IN THIS CONDITION???
Parent - By Tyrone (***) Date 12-11-2017 12:17
Okay, calm down.
STOP YELLING!!!

Welcome to the Original AWS Forum.
Hopefully someone with more ASME knowledge will get back to you soon.
Parent - By jwright650 (*****) Date 12-11-2017 17:33
Question #3, answer is no to AWS D1.1. The AWS Document would be AWS D1.6 for 316 to A36
Parent - By Ayman Malah Date 12-14-2017 06:18
Dear,

Regarding your questions, please found my following answers:

1. you can't find the answer here as you need to be trained for ASME 9. ''beside that you need to mention the welding processed''
2.Use SWPS for AWS d1.1