eslam soliman
Date
12-30-2017 06:31
hey guys, i have weld that inspected by rt and it already has defect and to be repaired, after repair is done the contract preform ut to inspect, is this accepted? and how can i find it in code, "asmeb31.1
By
Steelslinger
Date
01-01-2018 06:13
If its in the contract as you stated, then yes it's required.
As far as code reference:
ASME B31.1 (2016 is the one I have for reference) - 127.4.11 and Table 136.4
Topic
Welding Industry
/
Inspection & Qualification
/ RT Repair
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill