- - By jymar Date 02-01-2018 00:41
I'm reviewing the latest D17.1 spec and found they remove the distance requirement instead, spec mention determine by fabricator or qualified medical personnel.. So where should i look for the distance requirement?:confused:
Parent - By Mwccwi (***) Date 02-13-2018 18:47
You should review again in particular clauses  5.3.2, 5.3.2.1, 5.3.2.3