Not logged inAmerican Welding Society Forum
hi everyone,
can you guys explain what is single repair area and what is multiple repair area ? is their any specified size of this area ?
I assume you are referring to a specific code or welding standard. Can you give a hint as to which one it is?
Al
Actually I'm giving an exam of AWS CWI and in their BOOK OF SPECIMEN of part B they specified some criteria for repair and removal of defacts like for crack repairs
Is there a definition in the BoS defining the difference?
Al
No there is no defination shown in BoS