- - By Aman88 Date 03-01-2018 09:18
Hi Guys,

I would like to weld the above with TIG rods Er70S and had few questions in mind

- Is the consumable correct as weldabilty reference for 1040 is 8 and 4 for 250?
- Ideal preheat and interpass temperature?
-HT required post welding?

Thanks heaps !
Parent - By 803056 (*****) Date 03-01-2018 14:59
Since no code applies, you're good to go.