- - By abikoswara Date 03-10-2018 01:56 Edited 03-10-2018 02:00
Anyone ever made WPS with AWS D1.6 Code ???????? I'm very confused, because on the AWS D1.6 there's no rules about position for WPS, and AWS D1.6 very different with AWS D1.1, and how about Grup no, is it essensial ?????  essensial variable for WPS on the AWS D1.6 very different with AWS D1.1
thanks,
Please Explain
Parent - By 803056 (*****) Date 03-10-2018 14:33
Different code, different rules.

Position has little affect on the mechanical properties. The base metal doesn't know if it is welded flat or overhead. That a welder's skill and has nothing to do with metallurgy.

The base metals are grouped a little differently, but they are grouped as are the filler metals.