What is the difference between
Welding Procedure Datasheet and Welding Procedure Specification?
Welding Procedure Data Sheet (WPDS) referenced under CSA Standards for Canadian Welding Bureau Certification is equivalent to Welding Procedure Specification (WPS) referenced under other international welding codes and standards.